Titanium Grade 2 (Ti Gr 2) pipes and tubes are a popular choice in industries that require high strength, corrosion resistance, and lightweight materials. Titanium is known for its excellent resistance to corrosion, making it ideal for use in harsh environments such as chemical processing, marine, and aerospace applications.
Titanium Grade 2, also known as commercially pure titanium, offers a balance of good mechanical properties and formability. It is widely used in applications where both strength and resistance to corrosion are critical, including heat exchangers, pressure vessels, and piping systems in industries like oil and gas, automotive, and pharmaceuticals.
Titanium Gr 2 pipes and tubes are made from titanium alloys that are primarily composed of titanium with small amounts of other elements such as oxygen, carbon, and nitrogen. This composition gives Grade 2 titanium its excellent strength-to-weight ratio and remarkable resistance to corrosion in many environments, including seawater, chlorine, and acidic substances. One of the most notable features of Grade 2 titanium is its ability to withstand extreme temperatures without losing its structural integrity, making it suitable for both high-temperature and low-temperature applications.
The low density of titanium makes it ideal for applications where weight is a concern, especially in industries like aerospace where every gram counts. Furthermore, titanium Gr 2 is non-toxic, biocompatible, and has a high resistance to biofouling, which makes it an excellent choice for medical devices and implants. Titanium tubes and pipes are also highly durable and have a long service life, reducing maintenance costs over time.
Importers and stockists of Titanium Gr 2 pipes and tubes typically source their materials from reputable manufacturers who follow stringent quality control measures. This ensures that the titanium products are free from defects and can withstand the challenges of corrosion and wear. Suppliers also offer customization services, such as cutting, bending, and machining, to ensure the pipes and tubes fit the specific requirements of a given project or application.
| UNS No. | R50400 |
|---|---|
| Standard | Titanium Gr 2 Pipes & Tubes |
| Pipe Size | 1/8" NB to 36" NB |
| Schedule | SCH5, SCH10, SCH10S, SCH40, SCH40S, SCH80, SCH80S, SCH160, SCH160S, SCHXXS |
| Type | Seamless, Welded, EFW, Fabricated |
| Tube Size | 4mm od to 50mm od |
| Thickness | 0.3mm to 5mm thk |
| Length | 100mm to 6000mm, Custom Cut length |
| End | Plain End, Threaded end |
| Form | Round, Square, Triangle etc. |
| C | Fe | H | N | O | Ti |
|---|---|---|---|---|---|
| 0.1 | 0.2 | 0.015 | 0.03 | 0.18 | 99.5 |
| Grade | Tensile Strength | Yield Strength | Elongation at break |
|---|---|---|---|
| Titanium Gr 2 | 690 MPa | 310 MPa | 45% |