Hastelloy C276 sheet has the perfect combination of many strong alloys. These alloys are elite, which belongs to the iron family, and austenitic steel. Hastelloy C276 sheets display high-level corrosion fighting strength. Hastelloy C276 plates may be applied to ship parts, and container parts that prove they are immune to marine elements.
The marine environment can destroy the metal to a great extent. Hastelloy C276 plates work there efficiently. Hastelloy C276 coils can sustain chloride ion presence in climatic conditions. Many alloys get oxidized due to salty water, but Hastelloy C276 coils also function well in such conditions.
Hastelloy C276 is a nickel-molybdenum-chromium based alloy that comes with a sparse content of great quality tungsten. These combinations help to offer excellent corrosion resistance properties in harsh working environments. The availability of nickel and molybdenum in the Hastelloy C276 plates helps impart excellent pitting resistance to acids and crevice corrosion resistance in reducing environments.
Being prominent suppliers and stockists, Delta Superalloys maintains a comprehensive inventory of Hastelloy C276 round bars in various sizes, dimensions, and finishes. This ensures timely delivery of materials, even for urgent requirements. The company’s extensive distribution network allows it to serve clients across multiple regions seamlessly. Moreover, Delta Superalloys offers customized solutions, catering to the specific needs of industries ranging from oil and gas to pharmaceuticals.
Hastelloy is a nickel, molybdenum, and chromium alloy that is noted for its outstanding anticorrosive properties. It also has various additional qualities, such as ductility, flexibility, and durability, which make it a popular alloy for both industrial and residential applications. Hastelloy is classified into grades, which determine its strength and qualities.
| UNS No. | N10276 |
|---|---|
| Standard | Hastelloy C276 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C276 | 2.4819 | N10276 | 57.00 | 14.5 - 16.5 | 2.50 | 15.0 - 17.0 | 4.0 - 7.0 | - | - | - | - | 0.01 | 0.01 | 0.08 | 1.00 | W - 3 - 4.5 / V - 0.35 / P - 0.025 |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy C276 | 690 | 285 | 40 | 8.89 |