Hastelloy C276 wire is one of them fabricated with the best raw material. Hastelloy C276 wire is made out of C276 alloy, which is a most multipurpose alloy. It is a composite of nickel, tungsten, molybdenum, and chromium. Due to these elements, components made out of material grade C276 having enhanced resistivity against corrosion and other variety of industrial chemicals.
Nickel, tungsten, molybdenum, and chromium-based alloy made wire are weldable and can easily be formed. So whether you are using a gas tungsten arc, a gas metal arc, a shielded metal arc, this Hastelloy C276 wire can adapt to any manufacturing method. Because it naturally prevents the production of grain boundary precipitates.
It’s not always the case with other kinds of alloys. It makes C276 versatile and ideal wire for different situations where irregularly shaped wire is used in areas that would be extremely corrosive for normal wiring.
These Alloy C276 Coil Wire helps reduce defects on the rolls which is necessary to produce defect free galvanized steel for the automotive industry. Alloy C276 Wire had four times better corrosion resistance than the original material and 20 percent better than the other alloys at 150 Degree F to 200 Degree F.
Alloy C276 Wire has a more restricted composition for improved performance, where these improvements are of such significance that it has been widely patented throughout the world.Hastelloy C276 Wire is tested for this hydrofluoric acid pre – scrubber after the original material failed. Sleeved electro – galvanizing finishing rolls made of Hastelloy C276 Coil Wire.
| UNS No | N10276 |
|---|---|
| Standard | Hastelloy C276 Wires |
| Diameter | 0.1mm to 100mm |
| Length | 100mm to 6000mm, Custom Cut Length |
| Form | Filler Wire, Coil Wire, Wire, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C276 | 2.4819 | N10276 | 57.00 | 14.5 - 16.5 | 2.50 | 15.0 - 17.0 | 4.0 - 7.0 | - | - | - | - | 0.01 | 0.01 | 0.08 | 1.00 | W - 3 - 4.5 / V - 0.35 / P - 0.025 |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Hastelloy C276 | 690 | 285 | 40 | 8.89 |