Incoloy 800 round bars are an alloy of nickel, iron, and chromium that is known for its excellent resistance to oxidation, corrosion, and high-temperature environments. Manufactured with a combination of superior materials, Incoloy 800 is highly regarded in industries where heat resistance, structural integrity, and durability are paramount.
Delta Superalloys, a prominent name in the metal industry, specializes in offering high-quality Incoloy 800 round bars to meet the needs of various sectors, including petrochemical, power generation, aerospace, and more.The unique properties of Incoloy 800 make it an ideal choice for applications that require resistance to both oxidation and carburization. It is designed to withstand extreme temperatures, often ranging from 700°C to 1,100°C, without compromising its mechanical properties.
This ability to maintain its structural strength in such harsh conditions makes it highly sought after for use in heat exchangers, furnace components, and other high-temperature systems. Incoloy 800 also exhibits good resistance to stress corrosion cracking, which further enhances its reliability in demanding applications.
As leading importers, suppliers, stockists, and exporters of Incoloy 800 round bars, Delta Superalloys ensures that its products are available in a variety of sizes, grades, and specifications to suit the diverse requirements of its global clientele.Delta Superalloys serves as a stockist of Incoloy 800 round bars, ensuring prompt availability and quick delivery times to meet urgent requirements. This allows businesses to maintain uninterrupted production schedules, minimizing downtime and ensuring that projects stay on track.
The durability and versatility of Incoloy 800 round bars make them a popular choice for industries like chemical processing, where resistance to corrosive environments is crucial. Additionally, the alloy is often used in the production of equipment exposed to thermal cycling, such as boilers, steam generators, and various types of pressure vessels. As an experienced supplier, Delta Superalloys is able to provide customers with the right solutions to ensure that their operations run smoothly, efficiently, and safely.
| UNS No | N08800 |
|---|---|
| Standard | Incoloy 800 Round Bars |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm thickness |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Thickness | 1.6mm to 100mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Round Bar, Square Bar, Hex(A/F) Bar, Rectangle Bar, Billet, Ingot, Forging, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Incoloy 800 | 1.4876 | N08800 | 30.0 - 35.0 | 19.0 - 23.0 | - | - | 39.5 Min | 0.75 Max | - | 0.15 - 0.60 | 0.15 - 0.60 | 0.10 Max | 0.01 Max | 1.00 Max | 1.50 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Incoloy 800 | 515 | 210 | 30 | 7.94 |