Incoloy 800 wires, produced by Delta Superalloys, are a highly sought-after material in industries that demand high-performance alloys capable of withstanding extreme temperatures and corrosive environments. This versatile alloy, made primarily of nickel, iron, and chromium, offers exceptional resistance to oxidation, carburization, and high-temperature oxidation. Its remarkable properties make it ideal for applications in the chemical processing, power generation, and aerospace sectors.
Incoloy 800 is a superalloy that maintains its strength and integrity at elevated temperatures, making it an excellent choice for components exposed to prolonged heat and aggressive conditions. The alloy's excellent thermal stability and resistance to scaling and corrosion in a range of temperatures up to 1,100°F (593°C) are what make it a preferred choice for high-temperature applications.
Delta Superalloys, a leading supplier of Incoloy 800 wires, ensures that their products meet the highest standards of quality and reliability. Whether you're looking for Incoloy 800 wire for aerospace or power generation applications, their products offer unmatched resistance to oxidation and carburization, even under extreme conditions. The alloy’s ability to retain its mechanical properties at elevated temperatures ensures a longer service life, reducing the need for frequent replacements and increasing operational efficiency.
Incoloy 800 fittings are designed to connect, control, or regulate the flow of fluids in various systems, providing both structural integrity and corrosion resistance in high-temperature environments. These fittings, which include elbows, tees, reducers, and couplings, maintain their mechanical strength at temperatures exceeding 1000°F (540°C), making them ideal for applications in industries such as petrochemical, food processing, and nuclear power.
As one of the leading suppliers of high-quality Incoloy 800 wires, Delta Superalloys caters to a global network of importers, stockists, and distributors. They provide the alloy in various forms, including wires of different gauges and diameters, making it accessible for a wide range of industrial applications. These wires are distributed across many countries, ensuring that industries worldwide can benefit from the superior qualities of Incoloy 800.
| UNS No | N08800 |
|---|---|
| Standard | Incoloy 800 Wires |
| Diameter | 0.1mm to 100mm |
| Length | 100mm to 6000mm, Custom Cut Length |
| Form | Filler Wire, Coil Wire, Wire, etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Incoloy 800 | 1.4876 | N08800 | 30.0 - 35.0 | 19.0 - 23.0 | - | - | 39.5 Min | 0.75 Max | - | 0.15 - 0.60 | 0.15 - 0.60 | 0.10 Max | 0.01 Max | 1.00 Max | 1.50 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Incoloy 800 | 515 | 210 | 30 | 7.94 |