Alloy 800 is an austenitic steel, which is made with high concentrations of nickel. The Incoloy 800 Plate has a chemical composition of carbon, nickel, chromium, molybdenum, silicon, sulfur, copper, ferrous, aluminum, and titanium. These plates exhibit high corrosion and oxidation resistance in all types of mediums. Inconel 800 Sheet is designed with excellent mechanical properties.
These sheets have a minimum tensile strength of 520Mpa and a minimum yield strength of 205Mpa. The Inconel 800 Plate is highly versatile and widely used in thermal power plants, chemical industries, boilers, heat exchangers, condensers, nuclear fuel, and so on. We are the leading Incoloy 800 Plate supplier in the country. Our goal is to supply high-quality products, which are available at feasible rates for all.
The UNS N08800 Strip is designed with superior strength and enhanced creep resistance properties. These strips are available in thickness between 1000mm to 2500mm. UNS N08800 Shim Stock is used to provide structural support to various types of equipment in many industries. All our products are produced using cutting-edge technology and the best raw material following all industrial guidelines.
The Nickel Alloy 800 Hot Rolled Plate is produced by processing steel at high temperatures. These plates are very reliable and are known for their good dimensional accuracy. The DIN 1.4876 Cold Rolled Plate is formed after the hot-rolling process. These plates possess a superior surface finish and enhanced hardness and chemical make-up. They are also immune to acid-induced metal cracking. An AMS 5871 Polished Plate gives an aesthetic appearance to the observer due to its superior finish.
As a result, these plates provide extra protection in corrosive and oxidative mediums. All our products including, the Nickel Incoloy 800 Sheet, can be customized as per your requirements with desired chemical makeup, shapes, and sizes. If you have any questions about our products or want to get a quote on them, contact us.
| UNS No. | N08800 |
|---|---|
| Standard | Incoloy 800 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| length | 100mm to 6000mm, Custom Cut length |
| Forms | Coils, shims, plates, sheets, strips, flats. |
| finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| GRADE | Werks Toff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Incoloy 800 | 1.4876 | N08800 | 30.0 - 35.0 | 19.0 - 23.0 | - | - | 39.5 Min | 0.75 Max | - | 0.15 - 0.60 | 0.15 - 0.60 | 0.10 Max | 0.01 Max | 1.00 Max | 1.50 Max | - |
| Element | Tensile Strength Rm (Mpa) | Yield strength Rp0.2 (Mpa) | Elongation A5% | Density (g/cm3) |
|---|---|---|---|---|
| Incoloy 800 | 515 | 210 | 30 | 7.94 |